Shatter index of metallurgical coke on 2 inches and 0.5 inch screen should be respectively around _______________ percent?

Chemical Engineering Mcqs

Shatter index of metallurgical coke on 2 inches and 0.5 inch screen should be respectively around _______________ percent?

(A)  80 and 97

(B)  95 and 100

(C)  40 and 70

(D)  25 and 97